Brand Name : Rongsheng Xinwei
Model Number : Fused Cast α Corundum Bricks, Fused Cast β Corundum Bricks, Fused Cast α-β Corundum Bricks
Certification : ISO9001
Place of Origin : Zhengzhou ,China
MOQ : 1 Ton
Price : 200-800USD
Payment Terms : TT; L/C
Supply Ability : 2000tons /month
Delivery Time : 20-30DAYS
Packaging Details : packed on wooden pallets, with water-proof cover, and tightened with plastic/steel bandages
Al2O3 Content : ≥90%
Bending Strength : 200MPa
Color : Red
Compressive Strength : 300MPa
Density : 3.85g/cm3
Material : Corundum
Porosity : ≤20%
Product Name : Corundum Brick
Refractoriness : 1790℃
Refractoriness Under Load : 1450℃
Shape : Brick
Size : Customized
Softening Temperature : 1400℃
Thermal Conductivity : 1.2W/m.K
Thermal Expansion Coefficient : 4.5×10-6/K
Customized Fused Corundum Brick Kiln Fire Brick Wear-resistant Corundum Refractory Bricks For Industrial Furnace
Fused corundum bricks are highly sought-after due to their exceptional properties and are primarily composed of corundum as the main crystalline phase. The Alumina content of Fused Corundum Brick is greater than 90%, are the hot selling product of Rongsheng Group.
Applicaiton of Fused Corundum Brick
Fused corundum bricks are used in industries where extreme temperatures and corrosive environments are prevalent. Key applications include lining steelmaking furnaces, glass melting furnaces, ceramics kilns, chemical reactors, cement rotary kilns, non-ferrous metal furnaces, and power generation systems, among others. Their high compressive strength, resistance to acidic or alkaline substances, and ability to withstand temperatures over 1700°C make them indispensable in high-temperature industrial processes.
Parameters of Fused Corundum Brick
Item | Index | ||
Fused Cast α Corundum Bricks | Fused Cast β Corundum Bricks | Fused Cast α-β Corundum Bricks | |
Al2O3 % | 98 | 92 | 94.0 |
Na2O % | 1.0 | 6.5 | 4.0 |
SiO2+CaO+Fe2O3+TiO2 % | ≤1.0 | ≤1.5 | ≤2.0 |
α-Corundum % | 90 | 2 | 44 |
β-Corundum % | 4 | 97 | 55 |
Glass Phase % | 6 | 1 | 1 |
Bulk Density (Dense part) g/cm3 | 3.3 | 3.1 | 3.3 |
Cold Crushing Strength MPa | 200 | 50 | 200 |
0.2Mpa Refractoriness Under Load ℃ | 1700 | 1700 | / |
Static Resistance To Liquid Glass Erosion Depth mm/24h Ordinary Soda Lime Glass 1350℃×48h | / | / | 0.3 |